Grade |
Chemical Composition |
||||||||||
37SiMn2MoV |
The Element (%) |
||||||||||
C |
Si |
Mn |
Cr |
Mo |
Ni |
W |
B |
Al |
Ti |
V |
|
0.33-0.39 |
0.60-0.90 |
1.60-1.90 |
- |
0.40-0.50 |
- |
- |
- |
- |
- |
0.05-0.12 |
Grade |
Mechanical Property |
|||
37SiMn2MoV |
Yield Strength |
Tensile Strength |
Elongation |
Impact energy |
980 |
835 |
12 |
63 |
|
Grade 37SiMn2MoV steel is usually used in quenched and tempered condition. This alloy can be used after normalizing to make important parts such as shafts, small shafts, balance levers, etc. 37SiMn2MoV steel works under wear and friction conditions or under large impact loads. Rocker, connecting rod, bolt, nut, gear and various rollers. In addition, GB 3077 37SiMn2MoVsteel can also be used as a high-frequency surface hardening steel for parts requiring high surface hardness and wear resistance.