Products from DIN 17100 ST 44-2 steels are use in welded, riveted and screwed structural components. DIN 17100 ST 44-2 steels are not intended for heat treatment - apart from stress-relieving heat treatment and normalizing.
Grade |
thickness |
C |
P |
S |
N 2 |
ST44-2 |
16≤t≤40 |
0.24 |
0.060 |
0.060 |
0.010 |
40<t≤100 |
0.25 |
Grade |
Tensile strength |
Yield point |
|||||
ST44-2 |
t<3 |
3≤t≤100 |
t≤16 |
16<t≤40 |
40<t≤63 |
63<t≤80 |
80<t≤100 |
430-580 |
410-540 |
275 |
265 |
255 |
245 |
235 |
More information of DIN 17100 ST44-2 please contact Katalor to support you!