Products from
DIN 17100 ST 37-3 steels are use in welded, riveted and screwed structural components. DIN 17100 ST 37-3 steels are not intended for heat treatment - apart from stress-relieving heat treatment and normalizing.
DIN 17100 ST37-3 chemical composition
Grade |
C |
P |
S |
N 2 |
ST37-3 |
0.19 |
0.050 |
0.050 |
- |
DIN 17100 ST37-3 mechanical properties
Grade |
Tensile strength |
Yield point |
ST37-3 |
<3 |
≥3,≤100 |
≤16 |
>16,≤40 |
>40,≤63 |
>63,≤80 |
>80,≤100 |
360-510 |
340-470 |
235 |
225 |
215 |
215 |
215 |
DIN 17100 ST37-3 steels suitability for welding:
- Unlimited suitability of the DIN 17100 ST37-3 steels for the various welding processes cannot be guaranteed, since the behaviour of a steel during and after welding depends not only on the DIN 17100 ST37-3 material but also the conditions it experiences in manufacture and service.
- Suitability for flash butt-welding and gas pressure welding generally exists with all the steels of this Standard including DIN 17100 ST37-3, but it may be necessary in the case of steels with higher carbon content (ST50-2, ST60-2 & ST70-2) to carry out reheating after welding.
More information of DIN 17100 ST37-3 please contact Katalor to support you!