EN10025-2 S235JR Chemical Composition
Grade |
Chemical Composition |
||||||||
S235JR |
The Element Max (%) |
||||||||
C |
Si |
Mn |
P |
S |
N |
Cu |
|||
≤16 |
>16≤40 |
>40 |
|||||||
0.19 |
0.19 |
0.23 |
- |
1.50 |
0.045 |
0.045 |
0.014 |
0.60 |
EN10025-2 S235JR Mechanical Property
Grade |
Mechanical Property |
|||||||||||||
S235JR |
Yield Strength |
Tensile Strength |
||||||||||||
≤16 |
>16 |
>40 |
>63 |
>80 |
>100 |
>150 |
>200 |
>250 |
<3 |
≥ |
>100 |
>150 |
>250 |
|
235 |
225 |
215 |
215 |
215 |
195 |
185 |
175 |
- |
360-510 |
360-510 |
350-500 |
340-490 |
- |
S235JR is a grade under the Europe standard 10025-2. In the brand S235JR, S is the symbol for Structural Steel and JR for 20 temperature impac test, and a minimum yield strength of 235 N/mm²which can be widely used in the engineering and construction.
S235 material can be supplied in S235JR, S235J0, S235J2. The verification of the impact energy value should be carried out in accordance with EN 10025-1.