ASME SA283 Grade D Chemical Composition
Grade |
Chemical Composition |
|||||
A283 Grade D |
C |
Mn |
P |
S |
Si |
Cu |
≤0.27 |
≤0.9 |
≤0.030 |
≤0.030 |
0.15-0.4 |
≤0.2 |
ASME SA283 Grade D Mechanical Property
Grade |
Mechanical Property |
|||
SA283 Grade D |
Yield point min ksi[Mpa] |
Tensile strength ksi[Mpa] |
Elongation in 200mm (%) |
Elongation in 50mm |
60-80 |
33 |
20 |
23 |
ASTM A283GR. D is a kind of carbon steel plates of structural quality for general application. When the steel is to be welded, a welding procedure suitable for the grade of steel and intended use or service is to be utilized. See Appendix X3 of Specification A6/A6M for information on weldability.
In standard ASTM A283M, there are two types including plates of ASTM A283 Grade D and Grade C. As to the Chemical composition, the different content is a main on carbon content, while the carbon content of A283Gr. D is no more than 0.27% and it is higher than Grade C (≤0.24%) ; as to the mechanical property, the differences are tensile strength and yield strength, while the tensile strength of ASTM A283 Gr.D is 415-550MPa (60-80 ksi) and yield strength of ASTM A283 Grade D is 230MPa (33 ksi).