Steel Grade |
Chemical Composition % |
||||||
C |
Si |
Mn |
P |
S |
Cr |
Mo |
|
42CrMo |
0.38 to 0.45 |
0.17 to 0.37 |
0.50 to 0.80 |
≤ 0.030 |
≤ 0.030 |
0.90 to 1.20 |
0.15 to 0.25 |
Yield strength: ≥ 930 MPa
Tensile strength: ≥ 1080 MPa
Elongation: ≥12%
Rate of reduction in area: ≥45%
Impact absorbing energy: ≥ 63 J
Material Brinell hardness: ≤229 (Annealed or high temperature tempered steel rod)
Sample diameter: 25mm
Heat treatment specification
First quenching heating temperature: 850 °C (Cooling – oil)
Tempering heating temperature: 560 °C (Cooling – water, oil)